Sterling silver alloy and articles made from the same

STULLER, Inc.

US 10,697,044 B1GrantedGranted Jun 30, 2020Filed Nov 18, 2015

An improved sterling silver alloy. Like all sterlings, the improved alloy is at least 92.5 percent silver by weight. It has less copper than traditional sterlings: 3.0 percent versus the traditional 7.5 percent. Additionally, the improved alloy includes about 2.75 percent palladium, about 1.0 percent tin, and about 0.75 percent zinc, all by weight. A grain refiner, such as ruthenium, may also be provided. The components of the preferred alloy are melted, degassed, remelted, and then formed into casting grains, wire, and etc. The resulting alloy is significantly harder, as cast, than traditional sterlings: 95-120 Vickers versus 65 Vickers for traditional sterlings. The improved alloy also exhibits improved corrosion resistance. Other than a slightly higher (<200° F.) liquidus temperature, the improved alloy may be worked in substantially the same manner as traditional sterlings. Pieces…

Claims
3
1 independent claim
Filing to grant
4.6 years
Pendency
Earliest priority
2011
Sep 1, 2011
CPC classes
5
A44C · B22D · C22C

1ClaimsFirst of 3

  1. 1

    A method of making one or more jewelry articles comprising: placing a casting grains of an alloy in a crucible, wherein said alloy comprises at least 92.5 percent, by weight, silver; about 3.0 percent, by weight, copper; about 2.75 percent, by weight, palladium; about 1.0 percent, by weight, tin; and completely melting said casting grains by heating said crucible to a temperature of at least about 1790 degrees F.; pouring said molten alloy into an investment mold containing one or more jewelry…

2Description

Field of the Invention

The invention relates to sterling silver in general and hardened, corrosion resistant sterling silver in particular.